Model Number
G4001
Application Area
Dry lining
Plaster Depth
1 mm
Profile Wings
30x30 mm
Material
Galvanised Steel
Surface Treatment
Perforated embossed surface
Article number | Material Thickness | Standards | Lengths | Pack Qty. | Pallet Qty. | |
---|---|---|---|---|---|---|
add to List | G40015505 | 0.50 mm Z275 | EN 14353 | 200, 250, 260, 270, 275, 280, 300 cm | Pep: 25 pcs | 90 pep. |
add to List | G40011305 | 0.40 mm Z100 | EN 14353 | 200, 250, 260, 270, 275, 280, 300 cm | Pep: 25 pcs | 90 pep. |
Description
Used to joint on drywall edges. Provides a high-quality finish and solid protection at drywall corners. Minimizes cracking at the plasterboard edges.
Applications
- Suitable for interior applications.
- Not suitable for external applications unless secondary protection against corrosion is provided.
- Not permitted for areas exposed to high moisture and damp after application. (houses in wooded areas, wet rooms, swimming pools and domestic bathrooms etc.)
Compability
Suitable for lime, cement, lime-cement or gypsum-based plaster applications.
Materials
Manufactured with DX51D+Z galvanised steel strips with zinc coating in accordance to EN 10346.
- Z275 Zinc coating of 275 g/m 2 on both sides. Meets EN 13658 parts 1&2 and EN 14353 applications.
- Z100 Zinc coating of 100 g/m 2 on both sides Meets EN 14353 applications.
- Z60 Zinc coating of 60 g/m 2 on both sides. Meets no standard.
Installation
- Should be fixed with plaster or render dabs. Adhesive mortars with set accelerators containing chlorides are not suitable for fixing galvanised profiles.
- Not resistant to corrosion when using top coats of less than 3mm depth in exterior areas.
- Should not come into contact with aluminium or stainless steel profiles.
- Cut with hand plate shears across the wings and a fine toothed saw across bead noses.
- Should be fixed in accordance with embedding the bead’s wings into the plaster.
Notice !
Make sure that you choose the most suitable profile material and plaster mortar according to the application area to avoid excessive risks, claims and consequential damage. To prevent bimetallic corrosion, ensure that all metal components used in a given installation are of the same material type. Please ensure sufficient aeration to prevent corrosion and accelerate the drying time. Avoid damage to beads when trowelling plaster or render. Care should also be taken to prevent mechanical damage to the galvanised coating. The substrate must be dry, clean, dust-free, absorbent and load-bearing in accordance with the requirements of the plaster coats to be applied. The wall surface must not contain salts or foreign substances and efflorescence must be removed. In general, metal beads should be kept dry and stored flat.
Downloads
Description
Used to joint on drywall edges. Provides a high-quality finish and solid protection at drywall corners. Minimizes cracking at the plasterboard edges.
Applications
- Suitable for interior applications.
- Not suitable for external applications unless secondary protection against corrosion is provided.
- Not permitted for areas exposed to high moisture and damp after application. (houses in wooded areas, wet rooms, swimming pools and domestic bathrooms etc.)
Compability
Suitable for lime, cement, lime-cement or gypsum-based plaster applications.
Materials
Manufactured with DX51D+Z galvanised steel strips with zinc coating in accordance to EN 10346.
- Z275 Zinc coating of 275 g/m 2 on both sides. Meets EN 13658 parts 1&2 and EN 14353 applications.
- Z100 Zinc coating of 100 g/m 2 on both sides Meets EN 14353 applications.
- Z60 Zinc coating of 60 g/m 2 on both sides. Meets no standard.
Installation
- Should be fixed with plaster or render dabs. Adhesive mortars with set accelerators containing chlorides are not suitable for fixing galvanised profiles.
- Not resistant to corrosion when using top coats of less than 3mm depth in exterior areas.
- Should not come into contact with aluminium or stainless steel profiles.
- Cut with hand plate shears across the wings and a fine toothed saw across bead noses.
- Should be fixed in accordance with embedding the bead’s wings into the plaster.
Notice !
Make sure that you choose the most suitable profile material and plaster mortar according to the application area to avoid excessive risks, claims and consequential damage. To prevent bimetallic corrosion, ensure that all metal components used in a given installation are of the same material type. Please ensure sufficient aeration to prevent corrosion and accelerate the drying time. Avoid damage to beads when trowelling plaster or render. Care should also be taken to prevent mechanical damage to the galvanised coating. The substrate must be dry, clean, dust-free, absorbent and load-bearing in accordance with the requirements of the plaster coats to be applied. The wall surface must not contain salts or foreign substances and efflorescence must be removed. In general, metal beads should be kept dry and stored flat.
Downloads
item successfully added to your list.
G10105500
Galvanised Steel Corner Bead with PVC nose
0.50 mm | Z275 | Bundle | 2500 pcs